A brief study of delayed fracture in a seam-welded titanium panel is summarized in this memorandum. Examination of the fracture surface with electron microscopy
This memorandum represents a combined effort by the U.S. Naval Applied Science Laboratory, Brooklyn, New York, and the Defense Metals Information Center to summ
Porosity in fusion welds in titanium has been encountered to some extent in all programs using this joining method. While measures to control cleanliness and to